Researches on Normalizing Heat Treatment Applied to SAW Joints with TWIN-ARC

Article Preview

Abstract:

In this paper is analyzed the effect of normalizing post-weld heat treatment for SAW TWIN-ARC on grain size and aging of the Widmannstätten structure. Tests of elongation and toughness made with welded joints from S355J0 justify heat treatment opportunity and also the structural modification developed in deposited metal and in heat-affected zone.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

205-208

Citation:

Online since:

October 2007

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2007 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] G. Hochreiter: Unterpulverschweissen in der Praxis, Expert Verlag Rennigen-Malmsheim, (2005), pp.76-93.

Google Scholar

[2] A. Ya. Ishchenko, et al. The Paton Welding Journal, No. 1 (2002), p.10.

Google Scholar

[3] V. Ya. Kononenko, et. al. Avtomaticeskaia Svarka, part 5 (2004), p.25.

Google Scholar

[4] J. W. Mc Enerney: Soudage Tech. Connexes. Vol 53, (1999), p.12 Fig. 4 Micrographic image of the interface deposited metal - HAZ from a not treated weld (DM-HAZ 810x).

Google Scholar