Microstructure and Tensile Properties of Magnesium Alloy Containing Quasicrystallines Processed by Equal-Channel-Angular-Extrusion

Article Preview

Abstract:

Equal channel angular extrusion (ECAE) was performed on as-cast ZW1101 (Mg-11wt%Zn- 0.9wt%Y) Mg alloy containing quasicrystallines. The grain size of α-Mg was effectively refined, and coarse eutectic quasicrystalline phases were broken and dispersed in the alloy by ECAE. The alloy processed by ECAE exhibited a good combination of high strength and high ductility, which is due to the grain refinement and fine dispersed quasicrystallines in the alloy.

You might also be interested in these eBooks

Info:

Periodical:

Materials Science Forum (Volumes 475-479)

Pages:

469-472

Citation:

Online since:

January 2005

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2005 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] Z. P. Luo, S.Q. Zhang, Y. L. Tang and D. S. Tang: Scr. Metall. Vol. 28 (1993), P. 1513.

Google Scholar

[2] D. Shechtman, I. Bleach, D. Gratias and J.W. Cahn: Phy. Rev. Lett. Vol. 53(1984), P. (1951).

Google Scholar

[3] D. H. Bae, S. H. Kim, D.H. Kim and W. T. Kim: Acta Mater. Vol. 50 (2002), P. 2343.

Google Scholar

[4] S. Taniuchi, H. Watanabe, H. Okumura. S. kamado, Y. Kojima and Y. Kawamura: Mater. Sci. Forum, Vol. 419-422 (2003), P. 255.

DOI: 10.4028/www.scientific.net/msf.419-422.255

Google Scholar

[5] A. Singh, M. Nakamura, M. Watanabe, A. Kato and A. P. Tsai: Scr. Metall. Vol. 49 (2003), P. 417.

Google Scholar

[6] R. Z. Valiev, R. K. Islamgaliev and I.V. Alexandrov: Progress in Mater. Sci. Vol. 45 (2000), P. 103.

Google Scholar

[7] M. Mabuchi, K. Ameyama, H. Iwasaki and K. Higashi: Acta Mater. Vol. 47 (1999), P. (2047).

Google Scholar

[8] P. G. Partridge: Metall. Rev. Vol. 12 (1967), P. 169.

Google Scholar

[9] M. Y. Zheng, X. G. Qiao, S. W. Xu and K. Wu: Mater. Sci. Eng. A (submitted) Fig. 4 Stress-strain curves from the as-cast and ECAE processed ZW1101 alloy. Fig. 5 SEM fractograph of the 2-pass ECAE processed ZW1101 alloy. 0 2 4 6 8 10 12 14 16 18 0 50 100 150 200 250 300 As-cast 1P 2P 4P.

Google Scholar