Development of Thixoextrusion Process for 7000 Series Al Wrought Alloys

Article Preview

Abstract:

Thixoextrusion for 7003 and 7075 Al wrought alloys with different content of Cu was carried out with respect to isothermal holding temperature in the partially remelted semisolid state. Especially, despite higher extrudability index of 7075 Al wrought alloy compared with the extrudability index of 7003 Al wrought alloy, the maximum extrusion pressures of 7075 Al wrought alloy were about the same as the maximum extrusion pressures of 7003 Al wrought alloy at temperature with the liquid fraction 10% (7003-624, 7075-609). The hardness values of thixoextruded specimens were higher than that of as-quenched specimens only after partial remelting. The microstructures of thixoextruded specimens did not show any dendrites or rosette-like structures. The average grain sizes of thixoextruded specimens were smaller than average grain sizes of homogenized specimens.

You might also be interested in these eBooks

Info:

Periodical:

Solid State Phenomena (Volumes 116-117)

Pages:

771-774

Citation:

Online since:

October 2006

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2006 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] M.C. Fleming: Metall. Trans. Vol. A 22 (1991), p.957.

Google Scholar

[2] D.H. Kirkwood: Inter. Mater. Rev. Vol. 39 (1994), p.173.

Google Scholar

[3] G. Chiarmetta: Proc. 3rd Int. Conf. on Semi-Solid Processing of Alloys and Composites (1994), p.204.

Google Scholar

[4] K. Kiuchi and S. Sugiyama: Proc. 3rd Int. Conf. on Semi-Solid Processing of Alloys and Composites (1994), p.245.

Google Scholar