Paper Title:
Preparation of Refractory Castable for High-Temperature Zone of the Alumina Kiln
  Abstract

The cChromic shaped bricks have been used as the refractory lining in alumina kiln for long time, whose service life is about 120~250 days. Besides the short working time, the environmental pollution led to by the chromic component is also serious. In this thesispaper (thesis 是硕士论文), some materials are were chosen based on the actual situation of the usage of the refractory lining in the current alumina kiln. The choosing principals are were the extensive source and the relatively low price. Finally, a new formula of the refractory castable is was acquired based on the orthogonal test and has passed the properties testing.

  Info
Periodical
Advanced Materials Research (Volumes 217-218)
Edited by
Zhou Mark
Pages
1229-1234
DOI
10.4028/www.scientific.net/AMR.217-218.1229
Citation
X. X. Cao, J. G. Liao, X. F. He, L. L. Zhu, R. N. Wang, Q. Ma, "Preparation of Refractory Castable for High-Temperature Zone of the Alumina Kiln", Advanced Materials Research, Vols. 217-218, pp. 1229-1234, 2011
Online since
March 2011
Export
Price
$32.00
Share

In order to see related information, you need to Login.

In order to see related information, you need to Login.

Authors: Bing Qiang Li, Yao Shu, Wen Bin Dai, Jing Kun Yu
Chapter 3: Materials Engineering
Abstract:The effect of the zirconia, zirconite, and zircon mullite additives on the properties of alumina-spinel castable has been investigated in...
346
Authors: Qi Bing Chang, Ke Yang, Xia Wang, Ke Kai Cheng, Yong Qing Wang, Jian Er Zhou
Chapter 1: Raw Materials and Processing
Abstract:The high sintering temperature of Al2O3 is the main reason of the high cost of the common ceramic membrane supports. To...
56
Authors: Liang Qu, Mei Jie Zhang
Chapter 6: Physical Properties of Materials
Abstract:The heating furnace in CSP plant of WISCO has a lightweight lining which is built by all fiber templates. In light of its good thermal...