Models for the Porosity Growth and Dissolution in Single-Crystal Nickel-Base Superalloys
  Abstract

During the solidification and the homogenization of single-crystal nickel-base superalloys, pores form which lead to the degradation of the mechanical properties, especially the fatigue lifetime. Hot Isostatic Pressing (HIP) is used for the pores dissolution. In this paper, analytical models for the formation of the homogenization pores and their dissolution during the HIP are developed. The results are compared with experimental data.

  Info
Periodical
Defect and Diffusion Forum (Volumes 297-301)
Edited by
Andreas Öchsner, Graeme E. Murch, Ali Shokuhfar and João M.P.Q. Delgado
Pages
187-192
DOI
10.4028/www.scientific.net/DDF.297-301.187
Citation
B. S. Bokstein, V. Esin, A. O. Rodin, I.L. Svetlov, "Models for the Porosity Growth and Dissolution in Single-Crystal Nickel-Base Superalloys", Defect and Diffusion Forum, Vols. 297-301, pp. 187-192, 2010
Online since
April 2010
Export
Price
$32.00
Share

In order to see related information, you need to Login.

In order to see related information, you need to Login.

Authors: Yan Jun Li, Arild Håkonsen, Dag Mortensen, Tanja Pettersen, Trond Furu
Abstract:A simplified numerical model for the solid state phase transformation from Al6(Mn,Fe) to α-Al(Mn,Fe)Si phase in 3xxx alloys has been...
297
Authors: Ali Shokuhfar, Arash Rezaei, S.M.M. Hadavi, Shahram Ahmadi, H. Azimi
Abstract:Aluminum-Lithium alloys are attractive choices for weight saving of aerospace structures. By addition of Lithium to Aluminum alloys, the...
20
Authors: Romana Piat
Abstract:In the last years there has been an increasing interest in the multi-scale mechanics of the materials, i.e. in predicting the macroscopic...
665
Authors: Yong Zhi Zou, Zheng Bin Xu, Jian Min Zeng
Abstract:Aluminum alloy A357 can be heat treated in order to obtain optimum mechanical properties. Moreover, SDAS (Second dendrite arm spacing) is an...
1041
Authors: Li Zi He, Xie Hua Li, Jian Zhong Cui
Abstract:The microstructural evolutions of 7055 aluminum alloy after single and two-step homogenization with or without applying 12T high magnetic...
4472