Paper Title:
Fabrication of Porous Transpiration C/SiC Composites
  Abstract

A new technology, prefabricating pore media (PPM) technology that adopt glass fiber as pore media, for porous transpiration cooling C/SiC composites was studied. The result shows that the technology can control the pore structure successfully by the volume content and distribution of glass fiber in the braid, and the porous C/SiC composites have good bending strength above 300MPa.

  Info
Periodical
Key Engineering Materials (Volumes 368-372)
Edited by
Wei Pan and Jianghong Gong
Pages
1053-1055
DOI
10.4028/www.scientific.net/KEM.368-372.1053
Citation
H. L. Ji, C. R. Zhang, X. G. Zhou, Y. B. Cao, "Fabrication of Porous Transpiration C/SiC Composites", Key Engineering Materials, Vols. 368-372, pp. 1053-1055, 2008
Online since
February 2008
Export
Price
$32.00
Share

In order to see related information, you need to Login.

In order to see related information, you need to Login.

Authors: Dong Mei Zhu, Hong Na Du, Fa Luo, Wan Cheng Zhou
Abstract:Porous C/C composite with certain porosity prepared by Chemical vapor infiltration (CVI) was chosen as the preforms to develop the C/C-SiC...
1501
Authors: Xian Liang Zhou, Duo Sheng Li, Ai Hua Zou, Xiao Zhen Hua, Zhi Guo Ye, Qing Jun Chen
New Functional Materials
Abstract:SiCp/Al composites were fabricated by ceramic mold freedom infiltration and pressureless infiltration, respectively. The microstructure and...
658
Authors: Wan Chang Sun, He Jun Li, Qian Gang Fu, Shou Yang Zhang
Abstract:PAN-carbon fibers were pretreated using three methods. 2D-C/C composites were fabricated by a rapid chemical liquid-vaporized infiltration...
482
Authors: Cai Yun Yang, Xiu Ping Zan, Zhen Ying Hu, Jing Li
Chapter 1: Material Engineering and its Application
Abstract:Two different kinds of structural preforms were designed and manufactured, which were 3D layer-to-layer angle-interlock structure and 3D...
95
Authors: Xin Fan
Chapter 3: Micro/Nano Materials
Abstract:Blends of Poly(L-lactide) (PLLA) and nano-SiO2 powder were prepared via solution mixing. Effect of nano-SiO2 particles on the crystallinity...
367