Paper Title:
Effect of Heating Rate on Sintered Microstructure of W-Cu Nanocomposite Powder Produced Using W-CuO Mixture
  Abstract

The sintered microstructure homogeneity of W-15wt%Cu nanocomposite powders prepared from W-CuO mixture was investigated. The increment of heating rate considerably affected the homogeneity of sintered microstructure. In case of the higher heating rate, the microstructure was more homogeneous than that of the lower heating rate by reason of Cu- exudation during heating-up process.

  Info
Periodical
Materials Science Forum (Volumes 449-452)
Edited by
S.-G. Kang and T. Kobayashi
Pages
1125-1128
DOI
10.4028/www.scientific.net/MSF.449-452.1125
Citation
D. G. Kim, G. S. Kim, J. C. Kim, S. T. Oh, Y. D. Kim, "Effect of Heating Rate on Sintered Microstructure of W-Cu Nanocomposite Powder Produced Using W-CuO Mixture", Materials Science Forum, Vols. 449-452, pp. 1125-1128, 2004
Online since
March 2004
Export
Price
$32.00
Share

In order to see related information, you need to Login.

In order to see related information, you need to Login.

Authors: Sung Tag Oh, Se Joong Yoon
Abstract:The reduction behavior of Al2O3/CuO powder mixtures, prepared from Al2O3/CuO or Al2O3/Cu-nitrate, was investigated by using thermogravimetry...
181
Authors: Ke Pi Chen, Yong He, Dong Yu Liu, Zong De Liu
Abstract:CCTO powders were prepared by using molten salt method in the NaCl-KCl system. The effects of temperature and holding time on phase...
115
Authors: Jian Fang Qiao, Dan Dan Qin, Li Guan, Hai Long Wang, Rui Zhang
Abstract:CaCu3Ti4O12 (CCTO) barrier layer ceramic capacitor was prepared by a two-step sintering process. The CCTO powders were pre-synthesized at...
121
Authors: N.T. Chua, J. Wang, Jan Ma
Abstract:Lead-based piezoceramic, such as lead zirconate titanate (PZT), is widely used because it has excellent piezoelectric properties near the...
63
Authors: Bao Jian Fu, Ying Chun Zhang, Xiao Li Su, Yan Hong Liu, Ming Hong
Chapter 3: Electrical, Magnetic and Optical Ceramics
Abstract:MgTa2O6 powders with the tetragonal phase have been synthesized by mixed oxide method at 1100 °C when the molar ratios...
1222