Anomalous SWAXS Analysis of Zr-Cu-Ni-Al Quaternary Metallic Glass Joints |
|
| Journal | Materials Science Forum (Volumes 539 - 543) |
|---|---|
| Volume | THERMEC 2006 |
| Edited by | T. Chandra, K. Tsuzaki, M. Militzer , C. Ravindran |
| Pages | 2006-2011 |
| DOI | 10.4028/www.scientific.net/MSF.539-543.2006 |
| Citation | Hiroshi Okuda et al., 2007, Materials Science Forum, 539-543, 2006 |
| Online since | March, 2007 |
| Authors | Hiroshi Okuda, Isao Murase, Shojiro Ochiai, Yoshihiko Yokoyama, Katsuaki Inoue |
| Keywords | Anomalous Small-Angle Scattering, Anomalous Wide-Angle Scattering, Bulk Metallic Glass, Welding |
| Abstract | Anomalous small and wide angle scattering measurements on electron-beam welded joint has been carried out at Zr absorption edge. We preformed an anomalous and simultaneous small- and wide-angle scattering (A-SWAXS) analysis on the welded joint with and without crystallization. For the wide angle measurements, we extend the SAXS measurements up to 13 nm-1, where q is still below the first halo, but is large enough for several Bragg peaks to be observed. In the present analysis, the ASAXS analysis at the HAS/beads interface is interpreted in conjunction with the corresponding AWAXS analysis. The origin of SAXS and WAXS was found to be different. |
| Full Paper |
Get the full paper by clicking here
|