Paper Title:
Fabrication and Luminescence Properties of CaMoO4:Eu3+ Red Phosphors for White LED
  Abstract

CaMoO4: Eu3+ red phosphors were synthesized by co-precipitation method with H3BO3 as an additive and the relationship between H3BO3 doping amount and luminescent properties were studied. The brightness increased with increasing H3BO3 amount, the brightness of the CaMoO4: Eu3+ powder with 10 mol% H3BO3 was 3.2 times higher than that of the phosphor without H3BO3.

  Info
Periodical
Materials Science Forum (Volumes 663-665)
Edited by
Yuan Ming Huang
Pages
441-444
DOI
10.4028/www.scientific.net/MSF.663-665.441
Citation
Z. H. Liang, Y. Z. Feng, X. X. Liu, G. H. Peng, "Fabrication and Luminescence Properties of CaMoO4:Eu3+ Red Phosphors for White LED", Materials Science Forum, Vols. 663-665, pp. 441-444, 2011
Online since
November 2010
Export
Price
$32.00
Share

In order to see related information, you need to Login.

In order to see related information, you need to Login.

Authors: Li Qiong An, Jian Zhang, Min Liu, Sheng Wu Wang
Abstract:Yb3+ and Ho3+ co-doped Lu2O3 nanocrystalline powders were synthesized by a reversestrike co-precipitation method. The as-prepared powders...
521
Authors: Min Zhou, Cheng Zhang, Wen Bo Bu, Lei Wang, Qiang Li
Abstract:By means of co-precipitation, pure YAG phase was synthesized from the reaction of aluminum yttrium and cerium nitrates with ammonia as...
429
Authors: Rong Feng Guan, Qin Qin Li, Shuai Mou Li
Abstract:The YAG yellow phosphor was synthesized by Co-precipitation Method and its luminescent properties were characterized. The Orthogonal...
383
Authors: Xing Li, Jing Bao Lian
Abstract:A co-precipitation method for synthesizing Gd2O2S:(Yb3+,Er3+) nano-particles was developed, using the commercially available Gd2O3, Er2O3,...
546
Authors: Tao Han, Shi Xiu Cao, Ming Xing Ma, Da Chuan Zhu, Cong Zhao, Ming Jing Tu, Jin Zhang, Shi Yuan Zheng
Chapter 1: Material Science Technology
Abstract:YAG:Ce phosphors were synthesized by co-precipitation method. The photoluminescence intensity of samples sintered by the two-step route...
9