Abstract: The precipitation of T1 phase during the ageing of an Al- Li- Cu -Zr alloy sheet was studied by DSC (Differential Scanning Calorimetric) technique. Results showed that precipitation of T1 phase occurred in temperature range of 250°C to 300°C whereas its dissolution occurred within the temperature of 450°C to 530°C. Furthermore, activation energies for precipitation and dissolution of T1 phase were determined 122.1 kJ/mol and 130.3 kJ/mol, respectively.