Researches on Normalizing Heat Treatment Applied to SAW Joints with TWIN-ARC

Abstract:

Article Preview

In this paper is analyzed the effect of normalizing post-weld heat treatment for SAW TWIN-ARC on grain size and aging of the Widmannstätten structure. Tests of elongation and toughness made with welded joints from S355J0 justify heat treatment opportunity and also the structural modification developed in deposited metal and in heat-affected zone.

Info:

Periodical:

Edited by:

Ionel Chicinaş and Traian Canta

Pages:

205-208

Citation:

I. Mitelea et al., "Researches on Normalizing Heat Treatment Applied to SAW Joints with TWIN-ARC", Advanced Materials Research, Vol. 23, pp. 205-208, 2007

Online since:

October 2007

Export:

Price:

$38.00

[1] G. Hochreiter: Unterpulverschweissen in der Praxis, Expert Verlag Rennigen-Malmsheim, (2005), pp.76-93.

[2] A. Ya. Ishchenko, et al. The Paton Welding Journal, No. 1 (2002), p.10.

[3] V. Ya. Kononenko, et. al. Avtomaticeskaia Svarka, part 5 (2004), p.25.

[4] J. W. Mc Enerney: Soudage Tech. Connexes. Vol 53, (1999), p.12 Fig. 4 Micrographic image of the interface deposited metal - HAZ from a not treated weld (DM-HAZ 810x).

Fetching data from Crossref.
This may take some time to load.