Structure and Microwave Dielectric Properties of (Ca0.9375Sr0.0625)0.25 (Li0.5Sm0.5)0.75TiO3 Ceramics with B2O3-CuO Sintering Aids

Abstract:

Article Preview

The B2O3-CuO oxide mixture (abbreviated as BC) was selected to lower the sintering temperature of (Ca0.9375Sr0.0625)0.25(Li0.5Sm0.5)0.75TiO3 (abbreviated as CSLST) microwave dielectric ceramics by solid sate reaction technique. The effects of BC doping amounts on the crystal structure, microstructure and microwave dielectric properties of the ceramics were investigated. For the ceramic sample with the composition of CSLST + 5 wt% BC, its sintering temperature was reduced to 1000 °C as compared to 1200 °C for pure CSLST. In addition to the obtained good microwave dielectric properties as follows: εr = 80.4, Q×f = 1380 GHz, τf = -32.89 ×10-6/°C, this ceramic was a desirable high-permittivity microwave dielectric candidate for low-temperature cofired ceramic (LTCC) applications.

Info:

Periodical:

Advanced Materials Research (Volumes 284-286)

Main Theme:

Edited by:

Xiaoming Sang, Pengcheng Wang, Liqun Ai, Yungang Li and Jinglong Bu

Pages:

1442-1446

DOI:

10.4028/www.scientific.net/AMR.284-286.1442

Citation:

Y. M. Li et al., "Structure and Microwave Dielectric Properties of (Ca0.9375Sr0.0625)0.25 (Li0.5Sm0.5)0.75TiO3 Ceramics with B2O3-CuO Sintering Aids", Advanced Materials Research, Vols. 284-286, pp. 1442-1446, 2011