Research of Anticorrosion in Desulfurization Flue

Abstract:

Article Preview

Anti-corrosion coating in desulphurization flue of one wet flue gas desulfurization equipment (FGD) (model 1 and model 2) was designed and studied according to environmental and technical parameters of a coal-fired power plant. And relevant design requirements were confirmed. Application results showed that polyureas has wear and high temperature physical properties, so that it can be used in flue desulfurization equipment for anticorrosion. When the construction of a thickness of 2.0 mm, the high-temperature polyureas protective coating appearance smooth, EDM(electric discharge machining) 100% pass rate, adhesion 10.8 MPa, at 160 °C environment still had outstanding performance, that make sure it could reach its design life of the flue based on estimating the corrosion margin.

Info:

Periodical:

Advanced Materials Research (Volumes 301-303)

Edited by:

Riza Esa and Yanwen Wu

Pages:

462-466

Citation:

H. Zhu, "Research of Anticorrosion in Desulfurization Flue", Advanced Materials Research, Vols. 301-303, pp. 462-466, 2011

Online since:

July 2011

Authors:

Export:

Price:

$41.00

[1] Li Zhanyuan, Sun Yue, Yang Jianxin, Gao Peng, Zhuang Wenjun. Study on Using Hot Air For Heating Cleaned Flue Gas In Guohua Taishan Power Plant[J]. Thermal power generation. 2009, 37(9): 51-55(in Chinese).

[2] Wang Yingcong. Corrosion Of Equipment And Piping Used In Wet Desulphurization Device And Their Countermeasures[J]. Electric Power Construction. 2003, 24(10): 50-54(in Chinese).

[3] Wang Hairong, Zhang Haixin. Development Of Polyurea Elastomeric An Ti-Corrosion Coating[J]. Corrosion & Protection. 2006, 27(10): 529-531(in Chinese).

[4] Chen Suhong, Mu Hong. The stack anticorrosive material choice of No23 units in Baima Power Plant[J]. Electric Power Environmental Protection. 2008, 24(1): 25-27(in Chinese).

[5] Weng Zimao. Corrosion mechanism and protective material selection of desulfurizing equipment for flue gas in power plants[j]. Corrosion & protection. 2003, 24(5): 200-2057(in Chinese).

[6] Jiang Yuze. Corrosion Mechanism And Prevention For Flue Gas Cleanin G Equipment[J]. Corrosion & Protection. 2005, (26)12: 530-533(in Chinese).

[7] Hai Ni, Allen D. Skaja, Mark D. Soucek. _Acid-catalyzed moisture-curing polyurea/polysiloxane ceramer coatings[J]. Progress in Organic Coatings. 40 (2000): 175–184.

DOI: https://doi.org/10.1016/s0300-9440(00)00116-8

[8] Zeng Tinghua. Study on Influence of Wet Method Desulphurization System on Boiler Tail Flue Gas Duct and Stack[J]. 2002, 23(4): 19-22(in Chinese).

[9] Zhong Xin, Qian Jun, Geng Ningqing. Study on Anticorrosion Flame Plating Polyurea Elastomer[J]. Henan Chemical Industry. 2007,(24)2: 28-31(in Chinese).

[10] Liu Peili, Wang Baozhu, Hu Songxia, Liu Donghui, Xu Chunying. Study on Chemical Resistance of Aromatic Spray Polyurea Elastomer[J]. Paint & Coatings Industry. 2008, 38(11): 44-47(in Chinese).

[11] Zhang Qiang, Zhang Peipei, Jiao Qingze. Synthesis and Characterization of Microcapsules with Chlorpyrifos Cores and Polyurea Walls [J]. Chem. Res. Chinese U. 2006, 22(3): 379-382.

DOI: https://doi.org/10.1016/s1005-9040(06)60121-9

[12] Chen Xudong, Liu Lin, Wang Jiasheng. Study on the gelation time of spray polyurea elastomer. China Elastomerics. 2005, 15(5) : 15-l8 (in Chinese).