This Research Is to Study the High Strength Polyester Fabric Pre-treatment by Oxygen Plasma and Far-infrared, in the Rfl Chemical Solid Composition and Methylenediphenylisocyanate Concentration of 4% for Adding. Analysis Adhesion Strength between Fabric to Fabric and Fabric to Rubber of the Conveyor Belt, and the Effect of Pet Fabric Mechanical Properties. from the Result, the Best Treatment Condition Is Oxygen Plasma Treated 1min 120w and Add 4% Methylenediphenylisocyanate(mdi). in the Adhesion Strength of Fabric and Fabric Layer Compared with the Untreated Has Raised up to 21.5kgf (25.0%), and Fabric and Rubber Layer Has Raised up to 23.7kgf (55.9%). Heating 20 Seconds, after Stop 10 Seconds and then Heat 20 Seconds and Add 4% Methylenediphenylisocyanate(mdi) Fabric-fabric Adhesion Strength Is 13.4 Kgf, Fabric-rubber Adhesion Strength Is 15.8 Kgf, Fabric-fabric and Fabric-rubber Adhesion Strength that Improve 24.1%, 43.6%.

Info:

Periodical:

Advanced Materials Research (Volumes 332-334)

Edited by:

Xiaoming Qian and Huawu Liu

Pages:

295-298

DOI:

10.4028/www.scientific.net/AMR.332-334.295

Citation:

J. H. Hu et al., "Surface Interface Treatment of Conveyer Belt", Advanced Materials Research, Vols. 332-334, pp. 295-298, 2011

Online since:

September 2011

Export:

Price:

$35.00

In order to see related information, you need to Login.

In order to see related information, you need to Login.