Ln(Mg0.5Ti0.5)O3 (Ln=La, Nd, Sm) powders were prepared by polymeric precursor method. After calcined at the temperature range of 600 °C to 1300 °C, the powders were characterized by XRD, SEM and FT-IR. The results indicated that Ln(Mg0.5Ti0.5)O3 perovskite crystal phases were formed when the precursor powders were calcined at 800 °C and the crystallization of Ln(Mg0.5Ti0.5)O3 powders increased gradually with the increasing calcining temperature.

Info:

Periodical:

Advanced Materials Research (Volumes 335-336)

Edited by:

Yun-Hae Kim, Prasad Yarlagadda, Xiaodong Zhang and Zhijiu Ai

Pages:

940-943

DOI:

10.4028/www.scientific.net/AMR.335-336.940

Citation:

B. L. Liang et al., "Synthesis and Characterization of Ln(Mg0.5Ti0.5)O3 (Ln=La, Nd, Sm) Obtained by the Polymeric Precursor Method", Advanced Materials Research, Vols. 335-336, pp. 940-943, 2011

Online since:

September 2011

Export:

Price:

$35.00

In order to see related information, you need to Login.

In order to see related information, you need to Login.