Growth of Bi-Pb-Sr-Ca-Cu-O Films by Organic Chemical Spray Pyrolysis Deposition

Abstract:

Article Preview

Bi-Pb-Sr-Ca-Cu-O films were deposited at 270-420°C by organic chemical spray pyrolysis deposition with triphenyl bismuth (TPB), Pb(tmhd)2, Sr(tmhd)2, Ca(tmhd)2 and Cu(tmhd)2 (tmhd: 2,2,6,6-tetramethyl-3,5-heptanedione). A factorial experimental design was applied in order to study the interaction between composition, deposition temperature, annealing time and annealing temperature and the effect in the formation of crystalline phases. Results of their structural and chemical characterization are presented.

Info:

Periodical:

Edited by:

P. VINCENZINI and A. RIGAMONTI

Pages:

43-48

DOI:

10.4028/www.scientific.net/AST.47.43

Citation:

E. Díaz-Valdés et al., "Growth of Bi-Pb-Sr-Ca-Cu-O Films by Organic Chemical Spray Pyrolysis Deposition", Advances in Science and Technology, Vol. 47, pp. 43-48, 2006

Online since:

October 2006

Export:

Price:

$35.00

In order to see related information, you need to Login.

In order to see related information, you need to Login.