Pure and doped (Ca2+ or Sr2+) Bridgman crystals were studied at temperatures of between 250 and 580C. The enthalpy of migration of Li vacancies was estimated (table 112).
M.Sharon, R.R.Pradhananga: Journal of Solid State Chemistry, 1981, 40[1], 20-7
Table 112
Enthalpy of Migration of a Li Vacancy in Ca2+-Doped LiCl
Ca2+ (ppm) | Q (eV) |
0 | 0.61 |
207 | 0.64 |
407 | 0.55 |
675 | 0.60 |
929 | 0.56 |