The conductivity of polycrystalline spinels was measured, using alternating-current techniques, at temperatures of between 25 and 500C (table 122).

R.Kanno, Y.Takeda, O.Yamamoto: Materials Research Bulletin, 1981, 16[8], 999-1005

 

 

Table 122

Ionic Conductivity of Li2MnCl4

 

Temperature (C)

σ (S/cm)

Q (kJ/mol)

100-330

-

62

330-500

4.0 x 10-3(200C)

40

330-500

1.4 x 10-1(400C)

40