The conductivity was measured, at temperatures ranging from ambient to about 400K, by using an alternating-current impedance method. It was found that the conductivity obeyed an Arrhenius relationship. The conductivity at 120K, and the activation energy, were equal to 10-6S/m and 69kJ/mol.
Y.Furukawa, A.Sasaki, D.Nakamura: Solid State Ionics, 1990, 42[3-4], 223-6