An investigation was made of the Gorsky effect by using internal friction measurements at temperatures ranging from 110 to 930K. The diffusion behaviours within this temperature range were described by:
D: D (cm2/s) = 3.1 x 10-4 exp[-0.073(eV)/kT]
H: D (cm2/s) = 4.4 x 10-4 exp[-0.059(eV)/kT]
R.Cantelli, F.M.Mazzolai, M.Nuovo: Journal of the Physics and Chemistry of Solids, 1970, 31, 1811-7
Table 316
Diffusivity of 16O in V
Temperature (K) | D (m2/s) |
624 | 9.35 x 10-17 |
580 | 1.20 x 10-17 |
529 | 1.23 x 10-18 |
496 | 2.18 x 10-19 |