Layer-by-layer radiometric analyses, using 89Sr2+ tracers at between 750 and 1050C, were carried out on essentially non-porous material with a grain size of more than 0.001mm. The resultant effective diffusion coefficients could be described by:

D (cm2/s) = 8.5 x 10-1 exp[-210(kJ/mol)/RT]

M.V.Slinkina, G.I.Dontsov, A.G.Segalla: Izvestiya Akademii Nauk SSSR - Neorganicheskie Materialy, 1991, 27[9], 1997-9. (Inorganic Materials, 1991, 27[9], 1696-8)