By using a steady-state flow method, the diffusivities at 250 to 400C were found to be described by:
D (cm2/s) = 1.4 x 10-3 exp[-4.9(kJ/mol)/RT]
V.A.Kurakin, A.A.Kurdyumov, V.N.Lyasnikov, M.I.Potapov: Fizika Tverdogo Tela, 1979, 21[4], 1060-3
Table 10
Permeation of D in Au
Temperature (K) | D2 (MPa) | P (atom/msPa½) |
573 | 0.087 | 4.0 x 107 |
573 | 0.0054 | 3.2 x 107 |
373 | 88 | 8.1 x 101 |