It was found that the data for polycrystalline samples, at 770 to 950C, were described by:
D (cm2/s) = 2.78 x 10-1 exp[-43.39(kcal/mol)/RT]
V.N.Kaigorodov, S.M.Klotsman, A.N.Timofeev, I.S.Trakhtenberg: Fizika Metallov i Metallovedenie, 1968, 25[5], 910-23
The best linear fits to the solute diffusion data ([473] to [487], [517] to [528]) yield:
Ag: Ln[Do] = 0.33E – 15.5 (R2 = 0.73); O: Ln[Do] = 0.69E – 13.2 (R2 = 0.998);
O(l): Ln[Do] = 0.42E – 9.4 (R2 = 0.98)