Chronopotentiometric measurements were used to study the diffusion of Cd2+ ions in eutectic melts. The diffusivity of Cd2+ (0.023 to 0.024mol/l) at 450C was equal to 1.80 x 10-5cm2/s. The activation energy, at 390 to 530C, was 9.4kcal/mol.
Chronopotentiometry in Molten Chlorides. Application to the Study of the Electrochemical Properties of U and Pu in LiCl-KCl. A.Leseur: Commission d’Energie Atomique Report CEA-R-3793, 1969
Table 77
Diffusion of Np3+ in Molten LiCl-KCl Eutectic
Temperature (C) | D (cm2/s) |
400 | 4.60 x 10-6 |
450 | 7.10 x 10-6 |
500 | 1.08 x 10-5 |
550 | 1.44 x 10-5 |
600 | 2.04 x 10-5 |
650 | 2.69 x 10-5 |