Measuring the Devitrification of Bioactive Glasses


Article Preview



Key Engineering Materials (Volumes 254-256)

Main Theme:

Edited by:

Mário A. Barbosa, Fernando J. Monteiro, Rui Correia, Betty Leon




H. Arstila et al., "Measuring the Devitrification of Bioactive Glasses", Key Engineering Materials, Vols. 254-256, pp. 67-70, 2004

Online since:

December 2003




[1] H. Ylänen, K. H Karlsson, A. Itälä and H. T Aro: J. Non-Cryst Solids. Vol 275 (2000), p.107.

[2] O. Peitl Filho, G. P LaTorre and L. L Hench: J Biomed Mater Res. Vol. 30 (1996), p.509.

[3] A. El-Ghannam, E. Hamazawy and A. Yehia: J Biomed Mater Res. Vol. 55 (2000), p.387.

[4] P. Stoor, E. Söderling and J. I Salonen: Acta Odontol Scand. Vol. 56 (1998), p.161.

[5] M. Brink: Bioactive glasses with a large working range, Doctoral Thesis, Åbo Akademi University, Turku, Finland (1997).

[6] A. Itälä, J. Koort, H. O Ylänen, M. Hupa and H. T Aro: J Biomed Mater Res. In Press.

[7] L. Fröberg, L. Hupa and M. Hupa: Key Engineering Materials, accepted.