Mechanical Properties of Ceramic Laminates

Abstract:

Article Preview

The progress of research efforts on the mechanical properties of ceramic laminates is reviewed. Laminates with weak interface are described with respect to their failure mode and the criterions to achieve graceful failure. For laminates with strong interfaces basic principles concerning the residual stresses and their influence on crack propagation are introduced. The implications for strength, indentation strength, strength distributions, macroscopic R-curves and threshold strength are discussed.

Info:

Periodical:

Edited by:

Marc Anglada et al.

Pages:

87-96

Citation:

T. Lube, "Mechanical Properties of Ceramic Laminates", Key Engineering Materials, Vol. 333, pp. 87-96, 2007

Online since:

March 2007

Authors:

Export:

Price:

$38.00

[1] V.J. Laraia, A.H. Heuer: J. Am. Ceram. Soc. Vol. 72 (1989), p.2177.

[2] R.H. Doremus, Glass Science, (Wiley-Interscience, New York 1994).

[3] H.M. Chan: Annu. Rev. Mater. Sci. Vol. 27 (1997), p.249.

[4] W.J. Clegg, et al.: Nature Vol. 347 (1990), p.455.

[5] H. Liu, S.M. Hsu: J. Am. Ceram. Soc. Vol. 79 (1996), p.2452.

[6] J.R. Mawdsley, D. Kovar, J.W. Halloran: J. Am. Ceram. Soc. Vol. 83 (2000), p.802.

[7] E.J. Winn, I. -W. Chen: J. Am. Ceram. Soc. Vol. 83 (2000), p.3222.

[8] J. She, T. Inoue, K. Ueno: J. Eur. Ceram. Soc. Vol. 20 (2000), p.1771.

[9] K.S. Blanks, A. Kristoffersson, E. Carlström, W.J. Clegg: J. Eur. Ceram. Soc. Vol. 18 (1998), p. (1945).

[10] J.B. Davis, A. Kristoffersson, E. Carlström, W.J. Clegg: J. Am. Ceram. Soc. Vol. 83 (2000), p.2369.

[11] J. Ma, H. Wang, L. Weng, G.E.B. Tan: J. Eur. Ceram. Soc. Vol. 24 (2004), p.825.

[12] R.M. German, Sintering Theory and Practice, (Wiley, New York 1996).

[13] W.J. Clegg: Acta Metall. Mater. Vol. 40 (1992), p.3085.

[14] M. -Y. He, J.W. Hutchinson: Int. J. Solids Struct. Vol. 25 (1989), p.1053.

[15] A.J. Phillipps, W.J. Clegg, T.W. Clyne: Acta Metall. Mater. Vol. 41 (1993), p.805.

[16] C.A. Folsom, F.W. Zok, F.F. Lange: J. Am. Ceram. Soc. Vol. 77 (1994), p.689.

[17] M. -Y. He, J.W. Hutchinson: Trans. ASME Vol. 56 (1989), p.270.

[18] J. Abanto-Bueno, J. Lambros: Eng. Fract. Mech. Vol. 69 (2002), p.1695.

[19] A. Tarlazzi, et al.: Wear Vol. 244 (2000), p.29.

[20] R. Lakshminarayanan, D.K. Shetty, R.A. Cutler: J. Am. Ceram. Soc. Vol. 79 (1996), p.79.

[21] T. Chartier, T. Rouxel: J. Eur. Ceram. Soc. Vol. 17 (1997), p.299.

[22] P.Z. Cai, D.J. Green, G.L. Messing: J. Am. Ceram. Soc. Vol. 80 (1997), p. (1929).

[23] B. Hatton, P.S. Nicholson: J. Am. Ceram. Soc. Vol. 84 (2001), p.571.

[24] I.A. Gee, et al.: Adv. Appl. Ceram. Vol. 104 (2005), p.103.

[25] G. Blugan, et al.: Key Eng. Mat. Vol. 290 (2005), p.175.

[26] M. Lugovy, et al.: Acta Mat. Vol. 53 (2005), p.289.

[27] M.P. Rao, et al.: Science Vol. 286 (1999), p.102.

[28] M.G. Pontin, M.P. Rao, A.J. Sánchez-Herencia, F.F. Lange: J. Am. Ceram. Soc. Vol. 85 (2002), p.3041.

[29] R. Bermejo, et al.: Fatigue Fract. Engng. Mater. Struct. Vol. 29 (2006), p.71.

[30] N. Orlovskaya, et al.: J. Mat. Sci. Vol. 40 (2005), p.5483.

[31] C.J. Russo, M.P. Harmer, H.M. Chan, G.A. Miller: J. Am. Ceram. Soc. Vol. 75 (1992), p.3396.

[32] S. Bueno, R. Moreno, C. Baudin: J. Eur. Ceram. Soc. Vol. 25 (2005).

[33] K. -S. Cho, H. -J. Choi, J. -G. Lee, Y. -W. Kim: J. Mat. Sci. Vol. 36 (2001), p.2189.

[34] D. -S. Park, et al.: J. Eur. Ceram. Soc. Vol. 22 (2002), p.535.

[35] P.Z. Cai, D.J. Green, G.L. Messing: J. Am. Ceram. Soc. Vol. 80 (1997), p. (1940).

[36] A.J. Sánchez-Herencia, C. Pascual, J. He, F.F. Lange: J. Am. Ceram. Soc. Vol. 82 (1999), p.1512.

[37] S. Ho, C. Hillman, F.F. Lange, Z. Suo: J. Am. Ceram. Soc. Vol. 78 (1995), p.2353.

[38] M. -Y. He, A.G. Evans, J.W. Hutchinson: Int. J. Solids Struct. Vol. 31 (1994), p.3443.

[39] O. Prakash, P. Sarkar, P.S. Nicholson: J. Am. Ceram. Soc. Vol. 78 (1995), p.1125.

[40] M.P. Rao, F.F. Lange: J. Am. Ceram. Soc. Vol. 85 (2002), p.1222.

[41] M. Oechsner, C. Hillman, F.F. Lange: J. Eur. Ceram. Soc. Vol. 79 (1996), p.1834.

[42] B.D. Cullity, S.R. Stock, Elements of X-Ray Diffraction, (Prentice Hall, New Jersey 2001).

[43] K. Zeng, D.J. Rowcliffe: J. Am. Ceram. Soc. Vol. 77 (1994), p.524.

[44] G. De Portu, et al.: Comp. Sci. Tech. Vol. 65 (2005), p.1501.

[45] G. De Portu, S. Bueno, L. Micele, C. Baudin: J. Eur. Ceram. Soc. Vol. (in press 2006).

[46] C.R. Chen, et al.: Acta Mat. Vol. (submitted 2006).

[47] V. Sergo, D.M. Lipkin, G. de Portu, D.R. Clarke: J. Am. Ceram. Soc. Vol. 80 (1997), p.1633.

[48] A.V. Virkar, J.F. Jue, J.J. Hansen, R.A. Cutler: J. Am. Ceram. Soc. Vol. 71 (1988), p. C148.

[49] H.J. Oel, V.D. Frechette: J. Am. Ceram. Soc. Vol. 50 (1967), p.542.

[50] A.V. Virkar, J.L. Huang, R.A. Cutler: J. Am. Ceram. Soc. Vol. 70 (1987), p.164.

[51] R.A. Cutler, J.D. Bright, A.V. Virkar, D.K. Shetty: J. Am. Ceram. Soc. Vol. 70 (1987), p.714.

[52] P. Chantikul, G.R. Anstis, B.R. Lawn, D.B. Marshall: J. Am. Ceram. Soc. Vol. 64 (1981), p.539.

[53] J.J. Hansen, R.A. Cutler, D.K. Shetty, A.V. Virkar: J. Am. Ceram. Soc. Vol. 71 (1988), p. C501.

[54] P.Z. Cai, D.J. Green, G.L. Messing: J. Eur. Ceram. Soc. Vol. 18 (1998), p. (2025).

[55] R. Bermejo, et al.: J. Eur. Ceram. Soc. Vol. (in press 2006).

[56] V.M. Sglavo, M. Paternoster, M. Bertoldi: J. Am. Ceram. Soc. Vol. 88 (2005), p.2826.

[57] W. Weibull, A Statistical Theory of the Strength of Materials, (Generalstabens Litografiska Anstalts Förlag, Stockholm 1939).

[58] J. Pascual Herrero, F. Chalvet, T. Lube, G. de Portu: Mat. Sci. Forum Vol. 492-493 (2005), p.581.

DOI: https://doi.org/10.4028/www.scientific.net/msf.492-493.581

[59] S.L. Fok, B.C. Mitchell, J. Smart, B.J. Marsden: Eng. Fract. Mech. Vol. 68 (2001), p.1171.

[60] R. Tandon, D.J. Green: J. Am. Ceram. Soc. Vol. 74 (1991), p. (1981).

[61] H.F. Bueckner: Z. Angew. Math. Mech. Vol. 50 (1970), p.529.

[62] R.J. Moon, et al.: J. Am. Ceram. Soc. Vol. 85 (2002), p.1505.

[63] A.J. Blattner, R. Lakshminarayanan, D.K. Shetty: Eng. Fract. Mech. Vol. 68 (2001), p.1.

[64] J. Pascual, et al., Weight Function, J-Integral and Material Forces Approach to Apparent Toughness of Ceramic Multilayers, in: Proceedings of ECF16, Alexandropoulos, submitted (2006).

[65] T. Lube, J. Pascual Herrero, F. Chalvet, G. de Portu: J. Eur. Ceram. Soc. Vol. (in press 2006).

[66] J. Pascual, F. Chalvet, T. Lube, G. De Portu: Key Eng. Mat. Vol. 290 (2005), p.214.

[67] T. Fett, D. Munz, Stress Intensity Factors and Weight Functions, (Computational Mechanics Publications, Southampton 1997).

[68] T. Fett, D. Munz, Y.Y. Yang: Fatigue Fract. Engng. Mater. Struct. Vol. 23 (2000), p.191.

[69] N.K. Simha, et al.: Int. J. Fract. Vol. 135 (2005), p.73.

[70] M.P. Rao, J. Rödel, F.F. Lange: J. Am. Ceram. Soc. Vol. 84 (2001), p.2722.

[71] K. Hbaieb, R.M. McMeeking: Mech. Mat. Vol. 34 (2002), p.755.

[72] M.G. Pontin, F.F. Lange: J. Am. Ceram. Soc. Vol. 88 (2005), p.376.

[73] M. Lugovy, et al.: Comp. Sci. Tech. Vol. 62 (2002), p.819.

[74] D. Kovar, M.D. Thouless, J.W. Halloran: J. Am. Ceram. Soc. Vol. 81 (1998), p.1004.