Formation and Control of Burr in Grind-Hardening


Article Preview

Based on grind-hardening experiments, the two side-direction burrs were studied. Three main stages (burr generation, augmentation and formation) in the burr yielding process were clarified and the varying laws of burr morphologies and dimensions were systematically revealed. In turn raises, some new technologies, processes and methods of actively controlling burrs were put forward.



Key Engineering Materials (Volumes 359-360)

Edited by:

Jiuhua Xu, Xipeng Xu, Guangqi Cai and Renke Kang




G. C. Wang et al., "Formation and Control of Burr in Grind-Hardening ", Key Engineering Materials, Vols. 359-360, pp. 98-102, 2008

Online since:

November 2007




[1] L.K. Gillespie and P.T. Blotter: ASME, Vol. 98 (1976) No. 2, pp.66-74.

[2] F. Schafer: SME Paper MR, pp.75-483.

[3] N. Kazuo and A. Minori: Annals of the CRIP, Vol. 36 (1987) No. 1, pp.33-36.

[4] G.C. Wang, M. Arai and K. Nakayama: JSPE, (1987), pp.671-672.

[5] G.C. Wang: Metal Cutting Burrs (Jilin Press of Science and Technology, China 1997), pp.18-21. (In Chinese).

[6] G.C. Wang and C.Y. Zhang: Key Engineering Material, Vols. 259-260 (2004), pp.278-281.

[7] J.D. Liu: Study on the Forming Mechanism of the Grinding-Hardening Machining and Its Application Fundament (Ph.D. Dissertation, Jiangsu University, China 2005), pp.23-59. (In Chinese).

[8] J.D. Liu, G.C. Wang, K.M. Chen and Z.H. Jia: China Mechanical Engineering, Vol. 16 (2005) No. 11, pp.1013-1017. (In Chinese).

Fetching data from Crossref.
This may take some time to load.