Oxidation Resistance of 2D C/SiC Composites Fabricated by FCVI

Abstract:

Article Preview

Two-dimensional waved carbon fiber preforms were chemical vapor infiltrated under forced flow, thermal gradient mode for preparation of 2D C/SiC composites. In order to improve the oxidation resistance of the C/SiC composites, B4C powders were added into the preforms and aqueous silica sol-B4C compound coating was claded on the surfaces of composites. It was found that the oxidation resistance of 2D C/SiC composites at temperatures lower than 1273K was improved because of the formation of B2O3 and borosilicate glass by preventing the diffusion of oxygen.

Info:

Periodical:

Key Engineering Materials (Volumes 368-372)

Edited by:

Wei Pan and Jianghong Gong

Pages:

1056-1058

Citation:

C. P. Wang et al., "Oxidation Resistance of 2D C/SiC Composites Fabricated by FCVI", Key Engineering Materials, Vols. 368-372, pp. 1056-1058, 2008

Online since:

February 2008

Export:

Price:

$38.00

[1] J.E. Sheehan, et al.: Annu. Rev. Master. Sci, Vol. 24 (1994), p.19.

[2] P. Ehrburger, P. Baaranne and J. Lahaye: Carbon Vol. 24 (1986), p.496.

[3] D.W. Mckee, C.L. Spiro and E.J. Lamby: Carbon Vol. 26 (1984), p.507.

Fetching data from Crossref.
This may take some time to load.