Damage Mechanisms and Rupture Criterion of PM Ti-6Al-4V at 20K

Abstract:

Article Preview

A two parameters rupture criterion for Ti-6Al-4V is proposed, based on cryogenic rupture tests. microstructural observations and FEM analysis,. The damage mechanisms including the cavities nucleation process are analyzed. Moreover, the final steps of rupture are discussed with the help of the thermo-mechanical coupling mechanisms that are expected to operate at low temperatures.

Info:

Periodical:

Edited by:

Jaroslav Pokluda

Pages:

287-290

DOI:

10.4028/www.scientific.net/MSF.482.287

Citation:

S. Di Iorio et al., "Damage Mechanisms and Rupture Criterion of PM Ti-6Al-4V at 20K", Materials Science Forum, Vol. 482, pp. 287-290, 2005

Online since:

April 2005