Fabrication of Deep-Sub-Millimeter-Thick Compacts Using Spark Plasma Sintering

Article Preview

Abstract:

Nd-Fe-B type powder was sintered using spark plasma sintering method. Fabricated compact sintered at the temperature of 700 °C, is found to be a composite magnet with Nd-Fe-Co-B and α-Fe. The compact sintered at 700 °C shows slightly low coercivity and large remanent magnetization comparing to the compact sintered at 600 °C due to the formation of α-Fe phase, resulting in the large maximum energy product. Maximum energy product tends to decrease with decreasing thickness of sintered compacts below 0.5 mm in thickness.

You might also be interested in these eBooks

Info:

Periodical:

Materials Science Forum (Volumes 534-536)

Pages:

521-524

Citation:

Online since:

January 2007

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2007 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] M. Sagawa, S. Fujirama, H. Yamamoto and Y. Matsuura: J. Appl. Phys., Vol. 55 (1984) p. (2083).

Google Scholar

[2] J. J. Croat, J. F. Herbst, R. W. Lee and F. E. Pinkerton:J. Appl. Phys., Vol. 55 (1984) p. (2079).

Google Scholar

[3] M. Sagawa, S. Fujirama, H. Yamamoto and K. Hiraga: IEEE Trans. Magn., Vol. MAG-20 (1984), p.1584.

Google Scholar

[4] R. D. Brown and J. R. Cost : IEEE Trans. Magn., Vol. 20 (1989), p.3117.

Google Scholar

[5] D. N. Brown, M. Smith, B. M. Ma and P. Campbell: IEEE Trans. Magn., Vol. 40 (2004), p.2895.

Google Scholar

[6] V. Neu and L. Schults:J. Appl. Phys., Vol. 90 (2001) p.1540.

Google Scholar

[7] NEOMAX environmental sustainability report, (2005) p.26.

Google Scholar

[8] H. Ono, N. Waki, M. Shimada, T. Sugiyama, A. Fujiki, H. Yamamoto and M. Tani: IEEE Trans. Magn., Vol. 37 (2001) p.2552.

DOI: 10.1109/20.951232

Google Scholar

[9] T. Saito, T. Takeuchi and H. Kageyama: J. Appl. Phys., Vol. 97(2005) p. 10H103.

Google Scholar

[10] H. Ono, T. Tayu, N. Waki, T. Sugiyama, M. Shimada, M. Kanou, A. Fijiki, H. Yamamoto, K. Takasugi and M. Tani:J. Appl. Phys., Vol. 93(2003) p.4060.

DOI: 10.1063/1.1559639

Google Scholar

[11] K. Mori, R. Nakayama and K. Morimoto:J. Jpn. Soc. Pwder and Powder Metallurgy Vol. 52, (2005) p.700. Fig. 4 Thickness dependence of normalized maximum energy product for compact sintered at 700 ºC.

Google Scholar