Biocompatibility Evaluation of Lithium-Hydroxyapatite Composites

Article Preview

Abstract:

Fifteen different lithium-hydroxyapatite composites were tested in this work. LiHA were prepared using 0.25 %, 1 % and 2 % of lithium and five different sintering temperature 900, 1000, 1100, 1200 and 1300oC. Primary culture of osteoblasts were used to evaluate the biocompatibility of the samples, concerning to cell viability and alkaline phosphatase production. The 1% LiHA samples sintered at 1100, 1200 and 13000C showed the best results.

You might also be interested in these eBooks

Info:

Periodical:

Key Engineering Materials (Volumes 309-311)

Pages:

1121-1124

Citation:

Online since:

May 2006

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2006 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] L L Hench Bioceramics. J Am Ceram Soc. Vol 74 (1991), p.1487.

Google Scholar

[2] R Z Legeros. An introduction to bioceramics L. L. Hench. World Scientific Publication Singapure (1993).

Google Scholar

[3] J W Choi et al.: J. Am. Ceram. Soc. Vol 81 (1998), p.1743.

Google Scholar

[4] I Mayer et al.: Calcif. Tissue Int. Vol 38 (1986), pp.293-5.

Google Scholar

[5] SH Oh: J. Biomed Mater. Res. Vol 67A (2003), pp.104-11.

Google Scholar

[6] G Goller et al.: Key Engineering Materials. Vol 240-242 (2003).

Google Scholar