Papers by Author: Bong Young Ahn

Paper TitlePage

Abstract: The effects of the precipitate and martensite lath on the softening behavior have been investigated for 11Cr-3.5W-3Co steel during creep at 700. During creep, the precipitate on the PAG (prior austenite grain) boundaries and martensite lath boundaries coarsened. The recovery of dislocation density and an increase of martensite lath width took place. It is shown that the inverse of the size of the precipitates and the inverse of the square root of the martensite lath width have a linear relation with the Vickers hardness, which corresponds to the Hall-Petch relation and particle looping mechanism.
475
Abstract: Conventional eddy current bobbin probes, multi-pancake and/or rotating pancake probes, and transmit-receive eddy current probes are currently utilized in testing metal tubing. Each method has respective strengths and weaknesses. This paper proposes another eddy current probe with new features. The structure is designed to be sensitive to circumferential cracks, which are not easily detected with ordinary bobbin coil probes. The directions of the magnetic field and the eddy current around the coil were considered in design of the probe structure. Signals of these probes from the artificial defects were acquired and analyzed. Experimental results show that the developed probes are more sensitive to circumferential defects than comparable ordinary bobbin probes. In addition, the new probes are insensitive to axial defects. By employing both the new probes and ordinary bobbin probes, more reliable ECT can be performed.
505
Abstract: As cMUTs (capacitive Micromachined Ultrasonic Transducer) offer numerous advantages over traditional transducers in terms of efficiency, bandwidth, and cost, they are expected to replace piezoelectric transducers in many applications. In particular, 2D-array cMUTs have aroused great interest in the medical engineering society because of their ability to materialize a true volumetric ultrasonic image. In this study, single element cMUTs with 32 x 32 and 64 x 64 cells were successfully fabricated. The diameter and thickness of the membrane are 35  and 1000 nm, respectively, with a sacrificial layer thickness of 600 nm. The electric characteristics of the fabricated cMUT were measured. Tests on the efficiencies of the cMUT in terms of wave generation and in terms of detection according to the bias and pulse voltage were performed in an air atmosphere.
132
2225
Abstract: Several nondestructive evaluation methods were attempted for the estimation of the creep damage of degraded 2.25Cr-1Mo steel. The specimens of three different aging periods were prepared by an isothermal heat treatment at 430°C, 482°C, and 515°C. The effect of probe configuration on the electrical resistivity was studied. Single configuration method and dual-configuration method were utilized for measuring electrical resistivity. The electrical resistivity was determined by a standard DC four-point probe method at 24±0.5°C. Indentation test, magnetic characteristics test and ultrasonic test were carried out to investigate the correlation between the major characteristics and aging parameter. Unlike the electrical resistivity characteristics, ultrasonic attenuation coefficient and indentation characteristics did not show a relation to Larson-Miller parameter. However, a correlation between the electrical resistivity and aging parameter was identified, which allows one to estimate the extent of material degradation.
1951
619
606