Oxidation Resistance of 2D C/SiC Composites Fabricated by FCVI

Article Preview

Abstract:

Two-dimensional waved carbon fiber preforms were chemical vapor infiltrated under forced flow, thermal gradient mode for preparation of 2D C/SiC composites. In order to improve the oxidation resistance of the C/SiC composites, B4C powders were added into the preforms and aqueous silica sol-B4C compound coating was claded on the surfaces of composites. It was found that the oxidation resistance of 2D C/SiC composites at temperatures lower than 1273K was improved because of the formation of B2O3 and borosilicate glass by preventing the diffusion of oxygen.

You might also be interested in these eBooks

Info:

Periodical:

Key Engineering Materials (Volumes 368-372)

Pages:

1056-1058

Citation:

Online since:

February 2008

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2008 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] J.E. Sheehan, et al.: Annu. Rev. Master. Sci, Vol. 24 (1994), p.19.

Google Scholar

[2] P. Ehrburger, P. Baaranne and J. Lahaye: Carbon Vol. 24 (1986), p.496.

Google Scholar

[3] D.W. Mckee, C.L. Spiro and E.J. Lamby: Carbon Vol. 26 (1984), p.507.

Google Scholar