Papers by Keyword: Si:He

Paper TitlePage

Abstract: The effect of treatment at up to 1400 K (HT) under enhanced hydrostatic pressure (HP, up to 1.2 GPa) on helium implanted single crystalline silicon (Si:He, He ion dose up to 6x1017cm-2, energy up to 300 keV) has been investigated by transmission electron microscopy, secondary ion mass spectrometry, photoluminescence and X-Ray methods. The treatment of Si:He at ≤ 920 K - HP results in a formation of buried nano-structured layers containing helium filled cavities/bubbles and numerous extended defects; many less dislocations are created at ≥ 1270 K in Si:He treated under HP. HP affects the recrystallization of amorphous Si, diffusivity of implanted He and of implantation-induced defects and thus promotes the creation of more but smaller He-filled cavities/bubbles as well as other defects near the range of implanted He+.
285
291
229
Showing 1 to 3 of 3 Paper Titles