Tensile Behavior of 2.5D C/SiCN Composites

Article Preview

Abstract:

Tensile behavior of C fiber reinforced amorphous SiCN ceramic matrix composites (C/SiCN ) were investigated by tensile machine. The microstructure morphologies were observed by scanning electron microscope. The results indicate that the tensile stress-strain curves of C/SiCN composites dispaly typical elastic deformation and cracks propagation stages. The 1500°C pre-sabilization treatment of C/SiCN in vacuum facilitates room temperature tensile stress growth. The higher treated temperature such as 1900°C is yet opposite. The reasons were attributed to thermal stress relaxation of C/SiCN after pre-stabilization treatment in vacuum.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

67-70

Citation:

Online since:

November 2012

Authors:

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2012 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] L.C. Chen, K.H. Chen, S.L. Wei, P.D. Kichambare, J.J. Wu, T.R. Lu, C.T. Kuo, Thin Solid Films 355-356, (1999) 112-116.

DOI: 10.1016/s0040-6090(99)00490-3

Google Scholar

[2] L. An, R. Riedel, C. Konetschny, H-J. Kleebe, R. Raj, J. Am. Ceram. Soc. 81, (1998) 1349-1352.

Google Scholar

[3] D. Bahloul, P. Goursat, A. Lavedrine, J. Euro. Ceram. Soc. 11, (1993) 63-68.

Google Scholar

[4] L.A. Liew, W. Zhang, V.M. Bright, L. An, M.L. Dunn, R. Raj, Sensors and Actuators A 89, (2001) 64-70.

Google Scholar

[5] Qiao SR, Lu GF, Zhong JH, Zhang CY. Process for producing carbon/carbon silicon composites by electro-thermda24d3f5al pyrolysis. P.R. China patent ZL 2006 1 0043034.4, 2008.

Google Scholar

[6] Y Xia, SR Qiao,QQ Wang, CY Zhang. Advanced Materials Research 79-82 (2009) 1499

Google Scholar