The Synthesis and Morphology Control of High after-Grow Intensity SrAl2O4: Eu, Dy Phosphors

Article Preview

Abstract:

High after-grow intensity with controllable morphology SrAl2O4: Eu, Dy phosphors were synthesized by an innovative combustion-melted-salt-assistant-Sol-Gel (CMSASG) method, by using Oxides, Carbonate, Nitric acid, Polyethylene glycols and Urea as raw materials, Gel-forming at 100°C, Combustion under 450°C, Melted-salt-calcination at 1250°C. The luminescent intensity and after-grow intensity of the SrAl2O4: Eu, Dy phosphors with the suitable pair-dope synthesized by CMSASG method are higher than those of commercial samples. The size of the phosphor with excellent luminescent characteristics and shape of sphericity or near sphericity synthesized can be controlled from about 200 nm to 10 μm.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

678-681

Citation:

Online since:

November 2012

Authors:

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2012 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] Xubo Li, Qishu Huang, Yifeng Lei, et al.,: Materials Research and Application, Vol.5 (2011), p.82. (In Chinese)

Google Scholar

[2] Quanmao Yu, Xiaoxia Li, Xingdong Lv, et al., in: New Progress of Inorganic Luminescent Materials Research and Application, University of Science & Technology China Press, Hefei (2009). (In Chinese)

Google Scholar

[3] D. B. Bem, H. C.Swart: J Polymer Composites, Vol. 32 (2011), p.219.

Google Scholar

[4] JCPDS Card No. 34-0379.

Google Scholar

[5] Tianyou Peng,Huajun Liu,Huanping Yang,et al., : Materials Chemistry and Physics,Vol. 85 (2004),p.68.

Google Scholar