Beneficiation Process Optimization Study on a Low-Grade Hematite Ore

Article Preview

Abstract:

A hematite has low grade, fine disseminated size andcomplex disseminated relations, which are refractory iron ore. Using SLon pulsating high gradient magnetic separator, induction intensity 8500Oe, pulsating 20mm stroke, stroke of 120 beats / min), a crude iron ore concentrates a grade of 35.93.%, the recovery rate of 82.39% is obtained through high intensity magnetic separation.( The final iron concentrate with TFe grade of 64.83%,yield of 14.55% and iron recovery of 35.74% from the raw ores with TFe grade of 26.29% was obtained, with the first stage grinding size being 50% -0.074mm and the second stage,95% -0.074mm.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

2461-2464

Citation:

Online since:

February 2013

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2013 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] JunHui Zhang, Yuan Zhang, Metal Mine, No. 388, pp.60-62, October, (2008).

Google Scholar

[2] Wen Chen, Metal Mine, No. 407, pp.55-59, May, (2010).

Google Scholar

[3] Fengjun Shao, China Mining, Vol. 9, No. 9, pp.71-73, September, (2009).

Google Scholar

[4] Huanxiang Ma, Modern Mining, No. 413, pp.23-25, January, (2010).

Google Scholar

[5] Yumin Qin, Mining Metallurgy, Vol. 15, No. 3, pp.18-21, September, (2006).

Google Scholar