Influence of Fiber Volume Fraction and Aggregate Size on Flexural Behavior of High Strength Steel Fiber-Reinforced Concrete (SFRC)

Article Preview

Abstract:

The effects of aggregate size and fiber volume fraction on the flexural behavior of 70MPa high strength steel fiber-reinforced concrete (SFRC) were investigated in this work. Test variables consist of fiber volume fraction (0, 1 and 2 %) and maximum aggregate size (8, 13 and 20 mm). The prism for flexural test was 100 x 100 x 400 mm and was tested under four points loading. Flexural toughness index was measured using ASTM C 1018 procedure. Test results indicated that the addition of steel fiber to 70MPa high strength concrete improves flexural and post-cracking behaviors. This phenomenon is remarkable for SFRC mixture with higher fiber content and smaller aggregate size. Also, the flexural toughness of high strength SFRC depends primarily on fiber content. The maximum aggregate sizes were secondary in importance.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

223-226

Citation:

Online since:

August 2013

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2013 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] Nemkumar Bethia and Jean-Francois Trottier, ACI Materials Journal, (1992).

Google Scholar

[2] P. Balaguru and H. Najm, ACI Materials Journal, (2004).

Google Scholar

[3] B. Barr and M. R. Mohanad Noor, ACI Journal, (1985).

Google Scholar

[4] ASTM C 39-12 standard, ASTM, (2012).

Google Scholar

[5] ASTM C 1609-10 standard, ASTM, (2010).

Google Scholar

[6] ASTM C 1018-97 standard, ASTM, (1997).

Google Scholar