The Study on the Degreasing Technology of Silk Floss Treated with Leaching Method

Article Preview

Abstract:

Silk floss was deoiled with leaching Method using 6# light gasoline in order to improve wearability of silk floss. The effect of temperature, time and bath ratio on the oil removal efficiency was studied by single factor analysis method. The results showed that the optimum degreasing technologies of silk floss with 6# light gasoline are: bath ratio 1:30, treatment time 40 min, and treatment temperature 50 °C. Under the optimum degreasing technologies of silk floss, the residual oil ratio of silk floss is 0.01% which is far below national standard.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

114-117

Citation:

Online since:

January 2014

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2014 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] Z.H. Feng, L.J. Zhu, S.J. Min, J. Cai, J. Lv. Journal of Textile Research. 28(2007)22–25.

Google Scholar

[2] H.T. Lin, W.E. Ning, J.W. Huang, F. Jiang, Z.Y. Hu. Silk 2(2012)15–17.

Google Scholar

[3] J. Feng, J.H. Lao. Silk 5(1999)28–30.

Google Scholar

[4] Z.H. Feng, L.J. Zhu, S.J. Min, J. Cai, J. Lv. Silk 1(2007)34–37.

Google Scholar

[5] X.Y. Zhou, W.P. Zhu, Z.M. Bian. Silk 4(1994)41–44.

Google Scholar