Wear Resistance and XRD Analyses of CMoCuNiCrSiBO Coatings Obtained by Thermal Deposition on OLC45 Substrate

Article Preview

Abstract:

Idlers are machine elements which are subjected to friction solicitations. The geometry, dimensions and weight can’t be modified that is why we decided to modify the contact surface by coating. We have chosen the steel type OLC 45 and we coated it with CMoCuNiCrSiBO by thermal deposition. The selection of these materials was made after a detailed study of the literature. After we obtained the samples, we subjected them to qualitative analyses SEM and XRD and to Quantitative analysis – wearing – destructive test where we obtained the friction coefficient between two coated surfaces [1]. We made the samples which we have analyzed by X-Ray Diffraction and we obtained the quality of the coating [2]. The results showed that the new material has a better structure than the basic material, and we can estimate a high durability of the machine elements coated. On friction test we have determined friction coefficient value.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

10-15

Citation:

Online since:

October 2014

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2014 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

* - Corresponding Author

[1] C. Axinte, D-L. Chicet, I-L. Bistricianu, C. Munteanu., Materials specific to gears used in automotive industry. Bulletin of the Pollitechnic Institute of Iasi, (2010).

Google Scholar

[2] C. Axinte, C. Munteanu, A-C. Barbinta, E-S. Barca., Gears materials analysis in order to establish the mechanical properties, Bulletin of the Pollitechnic Institute of Iasi, Romania., (2010).

Google Scholar

[3] Information on http: /www. weld. labs. gov. cn.

Google Scholar

[4] B. Fulleringer, D. Nelias, Elasto-plastic layers of nonuniform thickness in contact mechanics, Proceedings of the Stle/Asme International Joint Tribology Conference, (2010).

DOI: 10.1115/ijtc2010-41217

Google Scholar

[5] J. Leroux, B. Fulleringer, D. Nélias, Contact analysis in presence of spherical inhomogeneities within a half-space., International Journal of Solids and Structures 47 (2010), 3034–3049.

DOI: 10.1016/j.ijsolstr.2010.07.006

Google Scholar

[6] Hoichen HesserTechnisches Zeichnen, Berlin., (2009).

Google Scholar

[7] D-L Chicet, I-L Bistricianu, C Axinte, C Munteanu., APS coating used to improve life of bearings., Bulletin of the Pollitechnic Institute of Iasi, (2010).

Google Scholar

[8] J.F. Matlik, High-frequency, high-temperature fretting-fatigue experiments, Wear, 261, (2006) 1367-1382.

DOI: 10.1016/j.wear.2006.03.048

Google Scholar