Burst Strength of Glass Fibre/Epoxy Composite Pipes Subjected to Impact Loading

Article Preview

Abstract:

The main objective of this experimental study was to investigate the effects of low velocity impact loading on the pressure bearing capacity of the E-glass/epoxy composite pipes. The pipes were produced by the conventional filament winding technique comprises of six axisymmetric layers with (±55°)3 winding angles. The specimens were impacted at three different energy levels which are 5 J, 7.5 J, and 10 J using an instrumented drop weight impact testing machine (IMATEK IM10). The samples were then filled with water and subjected to burst test until distinct leakage failure is observed. The results indicate that the peak force and contact time increases with increased of impact energy. For impacted samples, the pressure tests show that the burst strength of the pipes decreases with increase in energy levels during impact loading. During the burst tests, several damage types named leakage and eruption were observed.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

121-125

Citation:

Online since:

August 2015

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2015 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

* - Corresponding Author

[1] M. Quaresimin, M. Ricotta, L. Martello, S. Mian. Energy absorption in composite laminates under impact loading. Composite: Part B 44 (2013) 133-140.

DOI: 10.1016/j.compositesb.2012.06.020

Google Scholar

[2] D. J. Chang. Burst Tests of Filament-wound Graphite-epoxy Tubes. Journal of Composite Materials 37(9) (2003) 811-829.

DOI: 10.1177/002199803031032

Google Scholar

[3] S. A. Matemilola, W. J. Stronge. Low-speed impact damage in filament-wound CFRP composite pressure vessels. Journal of Pressure Vessel 119(4) (1997) 435–443.

DOI: 10.1115/1.2842327

Google Scholar

[4] H. Arikan. Failure Analysis of (±55°)3 Filament Wound Composite Pipes With An Inclined Surface Crack Under Static Internal Pressure. Composite Structure 92, (2010) 182-187.

DOI: 10.1016/j.compstruct.2009.07.027

Google Scholar

[5] A. Onder, O. Sayman, T. Dogan, N. Tarakcioglu. Burst failure load of composite pressure vessels. Composite Structures 89 (2009) 159-166.

DOI: 10.1016/j.compstruct.2008.06.021

Google Scholar

[6] M. S. Abdul Majid, T.A. Assaleh, A.G. Gibson, J.M. Hale, A. Fahrer, C.A.P. Rookus, M. Hekman. Ultimate elastic wall stress (UEWS) test of glass fibre reinforced epoxy (GRE) pipe. Composites: Part A 42 (2011) 1500–1508.

DOI: 10.1016/j.compositesa.2011.07.001

Google Scholar

[7] A. G. Gibson, M. S. Abdul Majid, T. A. Assaleh, J. M. Hale, A. Fahrer, C. A. P. Rookus and M. Hekman: Qualification and lifetime modelling of fibreglass pipe, Plast. Rubber Compos. 2011, 40, (2), 80–85.

DOI: 10.1179/174328911x12988622800972

Google Scholar

[8] ASTM D1599. Standard Test Method for Resistance to Short-Time Hydraulic Pressure of Plastic Pipe, Tubing, and Fittings. (2011).

DOI: 10.1520/d1599-99r11

Google Scholar