Contact Wear Studies over Idlers Sprayed with Ni Al Si Powder Using Atmospheric Plasma Spraying Method

Article Preview

Abstract:

In military and mining industry are many machine elements – in our case idlers (for tanks, conveyors, and any others machineries which are using transmissions system which are subjected of coverage with a high wear rezistance powder. These machine elements (idlers) must have high wear proprieties, because the functionality of the entire transmissions systems depends on them. Also the maintenance costs are very high, that is why we proposed to studies how to improve the performances of this machine elements. Researches in surface engineering allow the obtaining of new systems of materials by coating the basic material surface with other material having superior high wear properties. In order to improve the machine elements durability, wear resistance, friction, we proposed to obtain a new system of materials using Atmospheric Plasma Spraying – with Sulzer 9MCE equipment. We have chosen the steel type 34CrNiMo6, MOCN class, STAS 691 - 880 as basic material and we coated it with NiAlSi powder. We made the samples and we tested them. The analysis has been made with Tribometre, which produces some data which link us to a high wear rezistance.The NiAlSi coating deposited on steel substrate is dense and very tought. The results showed that the new material has a better microstructure than the basic material and its physical and mechanical properties have been improved.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

184-188

Citation:

Online since:

October 2014

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2014 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] Y.L. Yang, N. Guo, J.F. Li, Surf. Coat. Technol. 219 (2013) 1–7.

Google Scholar

[2] X.W. Qiu, Y.P. Zhang, L. He, C.G. Liu, J. Alloys Compd. 549 (2013) 195–199.

Google Scholar

[3] Petru Avram, Cătălina Axinte, Alexandru Bârcâ, Constantin Paulin, and Corneliu Munteanu, (2012), Thermal spraying coatings corrosion resistance on aggressive solution, Bulletin of the Pollitechnic Institute of Iasi, Romania.

Google Scholar

[4] J.F. Matlik, High-frequency, high-temperature fretting-fatigue experiments, (2006), Wear, 261, pp.1367-1382.

DOI: 10.1016/j.wear.2006.03.048

Google Scholar

[5] C. Guo, J.S. Zhou, J.M. Chen, J.R. Zhao, Y.J. Yu, H.D. Zhou, Surf. Coat. Technol. 205 (2010) 2142–2151.

Google Scholar

[6] I. Hemmati, V. Ocelík, J. Th.M. De Hosson, Surf. Coat. Technol. 205 (2011) 5235–5239.

Google Scholar

[7] B. Bax, C. Pauly, P. Leibenguth, K. Woll, F. Mücklich, Surf. Coat. Technol. 206 (2012) 3931–3937.

Google Scholar

[8] Virgil Geaman et al., Ni-5Al – Cladding by thermal arc spraying, Int. J of Modern Manufacturing Technologies, Vol. VI, No. 1, pp.55-58, (2014).

Google Scholar