The linear random isoprene-styrene copolymer (L-SIR) was prepared by solution polymerization with cyclohexane—n-hexane mixture as solvent and n-BuLi as initiator in the presence of the polar regulator—tetrahydrofuran (THF). Microstructures of L-SIR have been studied by 1H-NMR.

You might also be interested in these eBooks

Info:

Periodical:

Advanced Materials Research (Volumes 11-12)

Pages:

367-370

Citation:

Online since:

February 2006

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2006 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] D.C. Wang, Q. Liu and W. Li: Adhesion in China Vol. 23 (2002), p.23.

Google Scholar

[2] M. Morton and L.J. Fetters: Rubber Chem. Tech. Vol. 48 (1975), p.359.

Google Scholar

[3] D.C. Yang: Dissertation, Beijing University of Chemical Technology (1987).

Google Scholar

[4] J. Chen, C.F. He and G.T. Jin: China Synthetic Rubber Industry, Vol. 21 (1998), p.88.

Google Scholar

[5] Z.L. Yan, G.T. Jin, X. Wang and X.Y. Zhang: China Elastomerics, Vol. 11 (2001), p.12.

Google Scholar