Effect of Far-Infrared Pre-Heat Treatment and Adding Methylenediphenylisocyanate(MDI) on Adhesion Bonding between Reinforcement and Rubber of Conveyer Belt
Abstract:
This research of the PET/Nylon fabric pre-treatment by far-infrared and adding Methylenediphenylisocyanate(MDI) to 0%、2%、4%、6% and 8%. According to fabric absorption medicament effect and bonding strength content analyzing. Heating 20 seconds, after stop 10 seconds and then heat 20 seconds and add 8% Methylenediphenylisocyanate(MDI) is the beast treatment, fabric-fabric adhesion strength is 16.73 kgf, fabric-rubber adhesion strength is 18.70 kgf, fabric-fabric and fabric-rubber adhesion strength that improve 54.6%、69.6%.