Experimental Study on the Re-Bonded Magnesia - Zirconia Refractory for New Dry Process Cement Kiln

Article Preview

Abstract:

The use of magnesia-chrome refractories of the cement kiln can generate harmful hexavalent chromium in the environment and be hazardous to your health, so the study on the instead of magnesia-chrome refractories have become urgent issues. The raw material is made up of fused magnesite particles (particle size 0 to 3 mm), fine fused magnesite powder with the size less than 200 meshes and fine fused magnesia-zirconia’s powder with the size less than 320 meshes, polyvinyl alcohol and calcium lignosulfonate liquor being used as the combine. This paper discusses the effect of sinter temperature on sinter character of products.

You might also be interested in these eBooks

Info:

Periodical:

Advanced Materials Research (Volumes 287-290)

Pages:

823-826

Citation:

Online since:

July 2011

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2011 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] H.X. Li, J.X. Wang :Chinese cement, Vol.10 (2004), pp.79-82. (In Chinese)

Google Scholar

[2] H.J. Klischat et al: ZKG international , Vol.8 (1997), pp.14-16.

Google Scholar

[3] U.V. Bogers et al: World Cement, Vol.12 (1996), pp.26-27.

Google Scholar

[4] J. Ni:Friendly :Int . Cem . Reviem , Vol.9 (1996), pp.111-115.

Google Scholar

[5] M. Naziri : Int .Cem . Review , Vol.12 (1996), pp.176-179.

Google Scholar

[6] C.X. Wang Y.X. Zhang,Q.Y: Zircomia (ZrO2) composite, Vol.12(2003), pp.186-188. (In Chinese)

Google Scholar