Study on the Preparation and Properties of α-PbO2-CeO2-TiO2 Composite Material on Aluminum-Matrix

Article Preview

Abstract:

Composite α-PbO2 coatings with addition of different solid particles were prepared on A1/conductive coating electrodes in 4M NaOH solution with addition of PbO until saturation by electrochemical anode composite electrodeposition technology, doping with different TiO2 and CeO2 nanoparticles. The optimum formula and operating condition of the composite electrode material were obtained as follows: adding PbO solid to 4M NaOH until saturation, TiO2 15 g/L; CeO2 10g/L, temperature 40°C, current density 0.5A/dm2, electrodeposition time 4h. On this condition, the PbO2-(3.77wt%±0.4%)TiO2-(2.13wt%±0.4%)CeO2 composite coating can be obtained.

You might also be interested in these eBooks

Info:

Periodical:

Advanced Materials Research (Volumes 306-307)

Pages:

787-791

Citation:

Online since:

August 2011

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2011 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] H.T. Guo, S.Y. Zhang: Composite Coating, (Tianjin University Publications, China 1991).

Google Scholar

[2] I.H. Yeo, D.C. Johnson: J. Electrochem. Soc. Vol. 134 (1987), p.1973.

Google Scholar

[3] I.H. Yeo, S. Kim, R. Jacobson and D.C. Johnson: J. Electrochem. Soc. Vol. 136 (1989), p.1395.

Google Scholar

[4] R. Bertoncello, F. Furlanetto, P. Guerriero and M. Musiani: Electrochim. Acta Vol. 44 (1999), p.4061.

Google Scholar

[5] U. Casellato, S. Cattarin and M. Musiani: Electrochim. Acta Vol. 48 (2003), p.3991.

Google Scholar

[6] Z.C. Guo, CN. Patent 200810058194.5.(2008).

Google Scholar

[7] D. Devilliers, M.T. Dinh Thi and E. Mahé: Electrochim. Acta Vol. 48 (2003), p.4301.

Google Scholar

[8] J. Feng, D.C. Johnson: J. Appl. Electrochem. Vol. 20 (1990), p.116.

Google Scholar

[9] A.B. Velichenko, D. Devilliers: J. Fluorine Chem. Vol. 128 (2007), p.269.

Google Scholar