Preparation and Characterization of Heparin-Immobilized Poly(Ether Urethanes)
Abstract:
Heparin (Hep)-immobilized poly(ether urethanes) (PU) was prepared by a unique preparation procedure. Firstly, the poly(ether urethanes)(PU) containing diester groups in the side chains were synthesized. Then, PU was dispersed in aqueous solutions and immobilized with heparin after the hydrolysis of diester groups and carboxylation. The Fourier transform infrared spectroscopy (FTIR) and water contact angle (WCA) were used to characterize the heparin-bonded PU. The amount of heparin grafted on the PU was determined to be 0.57wt.% by the toluidine blue method. The heparin-immobilized PU could release just 12% of the immobilized heparin in the early 10 hours of the 70 hours immobilized heparin stability test.
Info:
Periodical:
Pages:
236-239
Citation:
Online since:
November 2011
Authors:
Price:
Сopyright:
© 2012 Trans Tech Publications Ltd. All Rights Reserved
Share:
Citation: