Study on Production of Burning-Free Brick Using Chinese Kuancheng Iron Ore Tailings

Article Preview

Abstract:

Based on the analysis of components of Chinese Kuancheng iron ore tailings, burning-free brick test block were produced using local iron ore tailings and blast furnace slag as raw material, portlant cement as mineral glue, and parget as mineral activator. The optimum formula and production process were obtained with experiment of compressive strength of test blocks. The optimum ratio of iron ore tailing to blast furnace slag is between 5:5 and 6:4, parget composition is between 6% and 8%, and cement usage can be reduced to 10%. After curing, burning-free brick compressive strength of 17.5Mpa can be reached without sandiness phenomenon, and performance far exceeds the M10 burning-free brick standards. The formula of burning-free brick proposed in this paper can solve the problem of mineral waste pollution in Kuancheng area

You might also be interested in these eBooks

Info:

Periodical:

Pages:

146-149

Citation:

Online since:

April 2012

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2012 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] Lin Lin Chen, Shen Hong Zhou: China Resources Comprehensive Utilization Vol. 11 (2005), pp.30-32.

Google Scholar

[2] Lu Liu, Wei Zheng, Cong Ling Zhu, Pan Li: Utilazation of Iron Ore Tailings in Building Materials, Resources & Industries Vol. 6 (2008), pp.60-62.

Google Scholar

[3] Shi Wei Huang, Yan Yan Li, Lin Cheng, Sheng Yan: Metal Mine Vol. 4 (2007), pp.81-84.

Google Scholar

[4] Jin Zhong Wang: Building Energy Efficiency Vol. 3 (2000), pp.27-30.

Google Scholar

[5] Jin Rui Zhang, Wen Ni, Qing Mei Jia: Metal Mine Vol. 3 (2007), pp.85-87.

Google Scholar