Experimental Research on Application of Tailings Mortar for Treatment of Copper-Nickel Acid Wastewater

Article Preview

Abstract:

The disposal of acid wastewater generated by a copper-nickel smelting enterprise by using abandoned tailings mortar combined with sulfide precipitation and coagulation indicated that this method has demonstrated good results: the effluent can acheive “Emmission standard of pollutants for copper, nickel, cobalt industry” (GB 25476-2010); the heavy metals in the sediment is not apt to experience dissolution, thus less possible for secondary pollution of soil and groundwater. The optimal combination conditions of this process for sludge/wastewater mass ratio is 14:1; sodium sulfide’s dosing is 20 ml, reaction time is 20 min; FeSO4 and acid waste water volum ratio is 0.05, the reaction time is 30 min.

You might also be interested in these eBooks

Info:

Periodical:

Advanced Materials Research (Volumes 634-638)

Pages:

218-224

Citation:

Online since:

January 2013

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2013 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] Z. H. Zou, S.F. He and C.Y. Han: Thechnology of Water Research. Vol. 36 (2010), pp.17-21. (In Chinese).

Google Scholar

[2] X. Zhang and H.Z. Zhang: China Mining Magazine. Vol. 21 (2012), pp.45-48. (In Chinese).

Google Scholar

[3] N. Kongsricharoern and C. Polprasert: Water Science and Technology, Vol. 31 (1995), pp.109-117.

Google Scholar

[4] E. L. Alison: Hydrometallurgy, Vol. 104 (2010), pp.222-234.

Google Scholar

[5] F. L. Fu and Q. Wang: Journal of Environmental Management, Vol. 92 (2011), pp.407-418.

Google Scholar

[6] Y.M. Sun and T. Hu: Shandong Chemical Industry, Vol. 37 (2008), pp.40-42. (In Chinese).

Google Scholar

[7] S. W. Wang and F.Y. Feng: Heavy metal waste water treatment(Published by Metallurgical Industry Press, China 1993).

Google Scholar

[8] L.P. Qiu and H.R. Liu: China Water and Wastewater, Vol. 16 (2000), pp.58-60. (In Chinese).

Google Scholar