Abstract:

Grade of fluorite in this test is 30.95%,containing CaCO3 0.86%. On the base of much experiment research, such as grinding fineness test, pH test, agent dosage test and so on, the optimum conditions were: grinding fineness for first stage is -0.074mm 65%,pH=9, sodium silicate 0.8 kg/t and oleic acid 0.7 kg/t . The result of tests showed that the grade of CaF2 concentrate, recovery and productivity are 95.38%, 63.42% and31.20% by adopting a circuit of one rough flotation and seven concentrating with grinding fineness -0.043mm90.3%.

You might also be interested in these eBooks

Info:

Periodical:

Advanced Materials Research (Volumes 652-654)

Pages:

2576-2579

Citation:

Online since:

January 2013

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2013 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] Liu Shuxian, Shen Lili, Niu Fusheng. Study on flotation process of low quality fluorite ore in hebei. Non-metallic Mines. 33(2010): 28-29(in Chinese).

Google Scholar